IIR

BASICALLY CHEMICAL STRUCTURE
Copolymer isobutylene /isoprene


GENERAL PROPERTIES
Specific weight of the compounds: 1,00 ÷ 1,55
Obtainable hardness Shore A or IRHD: 50 ÷ 70
Minimum temperature of use: -30°C ÷ -35°C * (-45°C) **
Maximum temperature of use: +110°C (+130°C) **

* depending from the types      ** with a specific optimal formulation

Download the PDF file

IIR

 

BASIC POLYMER HARDNESS

TECNOGOMMA
CODE

UTILIZATION TEMP.  (°C)

PARTICULAR CHARACTERISTICS AND APPROVALS

IIR
70

-30 / +120

Very high gas and air impermeability; very good dielectrical properties and excellent resistance at U.V. radiations. Good ozone resistance.
In compliance with FDA(177.2600-21) for food; indeterminate expire date.

 

Certified Productive DWGW Process

This is a work sheet issued by DVGW in addition to the EN 549 or EN 682 approvals for gas application in Germany market.

The work-sheet is subdivided in two parts:
The first one, which has already been obligatory in addition to EN 549 and EN 682 approvals, requires an identification test of the elastomeric material (through the IR technique).

The second one is still optional by now, and requires the following tests: Ozone resistance, Stress relaxation Tests, Compression set at condition of 3000 h at 70o C, with the surveillance of the compression set each 1000 h.

This test has the clearly intention to value the material behaviour in a quite significant time set. The maximum admitted compression set value has not been fixed. 